Yuhong Holding Group Co., LTD
| Tempat asal: | Cina |
| Nama merek: | YUHONG |
| Sertifikasi: | ABS, GL, DNV, NK, PED, AD2000, GOST9941-81, CCS, ISO 9001-2015 |
| Nomor model: | EN10216-5 UNS32205 |
| Kuantitas min Order: | 500kg |
|---|---|
| Harga: | Dapat dinegosiasikan |
| Kemasan rincian: | Kasing kayu lapis / Kasing Besi / Bundel dengan Tutup plastik |
| Waktu pengiriman: | 10-90 Hari |
| Syarat-syarat pembayaran: | L/C,T/T |
| Menyediakan kemampuan: | Sesuai Dengan Permintaan Klien |
| Standar: | EN10216-5 | Nilai: | UNS S32205 |
|---|---|---|---|
| Bahan: | Baja Tahan Karat dupleks | Diameter luar: | 1/8"-48" |
| Ketebalan Dinding: | SCH5S ke SCHXXS | Tipe: | Mulus |
| Akhir: | MENJADI/PE | Panjang: | 6m, 12m, atau sesuai kebutuhan |
| Menyoroti: | UNS32205 Tabung stainless steel dupleks,Industri kimia tabung stainless steel dupleks,EN 10216-5 pipa dupleks |
||
EN 10216-5 1.4462 UNS32205 Pipa Seamless Stainless Steel Duplex D3/T3 Standar Eropa
EN 10216-5 UNS32205 (Duplex Stainless Steel 2205) Pipa Seamless adalah material berkinerja tinggi dengan struktur duplex dari austenit dan ferit. Ia memiliki kekuatan tarik 750-850 MPa dan kekuatan luluh lebih dari 450 MPa, yang jauh lebih baik daripada baja tahan karat austenitik tradisional. Ia juga memiliki ketahanan yang sangat baik terhadap keretakan korosi tegangan klorida (SCC) dan pitting (PREN≥35), dan cocok untuk lingkungan yang keras seperti transportasi minyak dan gas (ketahanan terhadap korosi H₂S/CO₂), pipa bertekanan tinggi desalinasi, dan reaktor kimia.
Ia memiliki rentang ketahanan suhu yang luas (-50°C hingga 300°C), dan desainnya yang ringan dapat mengurangi ketebalan dinding, tetapi perlu mengontrol masukan panas pengelasan (bahan pengelasan ER2209 direkomendasikan) dan menghindari rentang rapuh 475°C. Ini adalah solusi tahan korosi yang efisien untuk menggantikan baja karbon atau baja tahan karat austenitik.
Pipa seamless EN 10216-5 UNS32205 didasarkan pada standar Eropa. Ia telah menjadi material pilihan untuk energi Eropa, teknik kimia dan kelautan melalui kekuatan tinggi, ketahanan korosi, dan kepatuhan lingkungan sepanjang siklus hidup. Pembuatan dan pengujiannya secara ketat mengikuti sistem EN/ISO untuk memastikan keandalan di bawah tekanan tinggi, korosi, dan suhu ekstrem. Ini adalah produk tolok ukur yang memenuhi tujuan pembangunan berkelanjutan industri UE.
| Nomor UNS Nilai Duplex |
Tipeb | C | Mn | P | S | Si | Cr | Ni | Mo | N | Cu | Lainnya |
| S31200 | ... | 0.030 | 2.00 | 0.045 | 0.030 | 1.00 | 24.0-26.0 | 5.5-6.5 | 1.20-2.00 | 0.14-0.20 | ... | ... |
| S31260 | ... | 0.03 | 1.00 | 0.030 | 0.030 | 0.75 | 24.0-26.0 | 5.5-7.5 | 2.5-3.5 | 0.10-0.20 | 0.20-0.80 | W0.10-0.20 |
| S31803 | ... | 0.030 | 2.00 | 0.030 | 0.020 | 1.00 | 21.0-23.0 | 4.5-6.5 | 2.5-3.5 | 0.08-0.20 | ... | |
| S32001 | ... | 0.030 | 4.0-6.0 | 0.040 | 0.030 | 1.00 | 22.0-23.0 | 1.00-3.00 | 0.60 | 0.05-0.17 | 1.00 | |
| S32205 | S31803 / S32205 | 0.030 | 2.00 | 0.030 | 0.020 | 1.00 | 19.5-21.5 | 4.5-6.5 | 3.0-3.5 | 0.14-0.20 | ... | |
| S32304 | 2304 | 0.030 | 2.50 | 0.040 | 0.030 | 1.00 | 21.5-24.5 | 3.0-5.5 | 0.05-0.60 | 0.05-0.20 | 0.05-0.60 | |
| S32520 | ... | 0.030 | 1.50 | 0.035 | 0.020 | 0.80 | 24.0-26.0 | 5.5-8.0 | 3.0-4.0 | 0.20-0.35 | 0.50-2.00 | |
| S32550 | 255 | 0.04 | 1.50 | 0.040 | 0.030 | 1.00 | 24.0-27.0 | 4.5-6.5 | 2.9-3.9 | 0.10-0.25 | 1.5-2.5 | |
| S32750 | 2507 | 0.030 | 1.20 | 0.035 | 0.020 | 0.80 | 24.0-26.0 | 6.0-8.0 | 3.0-5.0 | 0.24-0.32 | 0.50 | |
| S32760 | ... | 0.030 | 1.00 | 0.030 | 0.010 | 1.00 | 24.0-26.0 | 6.0-8.0 | 3.0-4.0 | 0.20-0.30 | 0.50-1.00 | c |
| S32900 | 329d | 0.06 | 1.00 | 0.040 | 0.030 | 0.75 | 23.0-28.0 | 2.5-5.0 | 1.0-2.0 | ... | ... | |
| S32950 | ... | 0.03 | 2.00 | 0.035 |
| UNS | Kekuatan Tarik (MPa) min |
Kekuatan Luluh 0.2% Bukti (MPa) min |
Perpanjangan (% dalam 50mm) min |
Kekerasan | |
| Rockwell C (HR C) | Brinell (HB) | ||||
| 782 | 621 | 448 | 25 | 31 maks | 293 maks |
| UNS | Kepadatan (kg/m3) |
Elastis Modulus(GPa) |
Koefisien Rata-rata Termal Ekspansi (μm/m/°C) |
Termal Konduktivitas (W/m.K) |
Panas Spesifik 0-100°C( J/kg.K) Listrik |
Resistivitas (nΩ.m) 0-100°C |
|||
| 0-315°C | 0-538°C | pada 100°C | pada 500°C | UNS S31803 / 2205 | |||||
| 782 | 190 | 13.7 | 14.2 | - | 1.4462 | - | 1.4462 | 850 | Perbandingan Spesifikasi Grade |
| UNS |
Tidak British Lama |
Euronorm | SS Swedia | JIS Jepang | BS | ||
|---|---|---|---|---|---|---|---|
| En | Tidak | Nama | 2205 | ||||
| S31803 / S32205 | 318S13 | - | 1.4462 | X2CrNiMoN22-5-3 | 2377 | SUS 329J3L | Aplikasi |
1. Teknik kelautan dan minyak dan gas (aplikasi inti Eropa)
2. Kimia dan farmasi (kepatuhan REACH/ROHS)
3. Transformasi energi dan rendah karbon
4. Transit kereta api dan kapal
![]()
Kontak Person: Nirit
Tel: +8613625745622
Faks: 0086-574-88017980