Yuhong Holding Group Co., LTD
Tempat asal: | Cina |
Nama merek: | YUHONG HOLING |
Sertifikasi: | ABS, GL, DNV, NK, PED, AD2000, GOST9941-81, CCS, ISO 9001-2008 |
Nomor model: | INCOLOY800, INCOLOY 800H, INCOLOY 800HT, INCOLOY 825 |
Kuantitas min Order: | 100KGS |
---|---|
Harga: | Negotiable |
Kemasan rincian: | Kayu lapis /Iron kasus kasus / bundel dengan plastik Cap |
Waktu pengiriman: | 10-15 hari |
Syarat-syarat pembayaran: | L/C, T/T |
Menyediakan kemampuan: | 1500 ton per bulan |
Standar: | ASTM B 163 / ASTM B 704 | Bahan: | INCOLOY800, INCOLOY 800H , INCOLOY 800HT, INCOLOY 825 |
---|---|---|---|
NDT: | UJI ARUS PUSAT, UJI HIDROSTATIK, | Kemasan: | Kasing kayu lapis / Kasing Besi / Bundel dengan Tutup plastik |
Jenis: | Tanpa jahitan | ||
Cahaya Tinggi: | Alloy Steel Seamless Pipe,Nikel Alloy Tabung |
ASTM B 163 ASTM B 407 Nikel paduan incoloy 825 Tubo sem costura Nikel paduan pipa 100% ET E HT
Incoloy Alloy 825
Nama perdagangan umum: Incoloy 825, Alloy 825, Nickelvac 825, Nicrofer 4241.
INCOLOY alloy 825 (UNS N08825, W.Nr. 2.4858) adalah paduan nikel-besi-kromium dengan penambahan molibdenum, tembaga, dan titanium.
Nikel, bersama dengan molibdenum dan
tembaga, juga memberikan ketahanan yang luar biasa terhadap lingkungan yang mengurangi seperti yang mengandung belerang dan
Molibdenum juga membantu ketahanan terhadap korosi lubang dan celah.
Kandungan kromium memberikan ketahanan terhadap berbagai zat oksidasi seperti asam nitrat, nitrat dan
Tambahan titanium berfungsi, dengan perawatan panas yang tepat, untuk menstabilkan paduan terhadap
sensitisasi terhadap korosi intergranular.
Spesifikasi
INCOLOY Alloy 825 ditunjuk sebagai UNS N08825 dan Werkstoff Number 2.4858. Ini tercantum dalam NACE
MR0175 untuk layanan minyak dan gas.
Batang, batang, kawat dan bahan tempa: BS 3076NA16, ASTM B 425, ASTM B 564, ASME SB 425, ASME
SB 564, ASME Code Case N-572, DIN 17752, DIN 17753, DIN 17754, VdTÜV 432, ISO 9723, ISO 9724,
ISO 9725.
Plat, lembaran dan pita: BS 3072NA16, BS 3073NA16, ASTM B 424, ASTM B 906, ASME SB 424, ASME
SB 906, DIN 17750, VdTÜV 432, ISO 6208.
Pipa dan tabung: BS 3074NA16, ASTM B 163, ASTM B 423, ASTM B 704, ASTM B 705, ASTM B 751,
ASTM B 775, ASTM B 829, ASME SB 163, ASME SB 423, ASME SB 704, ASME SB 705, ASME SB 751,
ASME SB 775, ASME SB 829, ASME Code Case 1936, DIN 17751, VdTÜV 432, ISO 6207.
lainnya: ASTM B 366, ASME SB 366, DIN 17744
Komposisi Kimia
Nikel........................................................................................................................................................................................................................38.0-46.0
Besi...........................................................................................................................................................................................................................................................................................................................................................................................................................................................................................................................................................................................................................................................................................................................................................................22.0 menit.
Kromium.....................................................................................................................................................................................................................19.5-23.5
Molibdenum.............................................................................................. yang dapat digunakan sebagai bahan baku untuk pembuatan bahan baku2.5-3.5
Tembaga1.5-3.0
Titanium.........................................................................................................................................................................................................................................................................................................................................................................................................................................................................................................................................................................................................................................................................................................................................................0.6-1.2
Karbon0.05 maksimal.
Mangan1.0 max.
Sulfur..............................................................................................................................................................................................................................................................................................................................................................................................................................................................................................................................................................................................................................................................................................................................0.03 max.
Silikon0.5 max.
Aluminium..........................................................................................................................................................................................................................................................................................................................................................................................................................................................................................................................................................................................................................................................................................0.2 maksimal.
INCOLOY 825 tabung tanpa jahitan |
Incoloy alloy 825 adalah paduan nikel-besi-kromium dengan penambahan tembaga, molibdenum dan titanium.Komposisi kimia paduan ini dirancang untuk memberikan ketahanan yang luar biasa terhadap banyak lingkungan korosifKandungan nikel yang cukup untuk ketahanan terhadap korosi tekanan ion klorida retak. nikel, bersama dengan molibdenum dan tembaga,juga memberikan ketahanan yang luar biasa terhadap lingkungan reduksi seperti yang mengandung asam sulfat dan fosforMolibdenum juga membantu ketahanan terhadap korosi lubang dan celah.asam nitrat dan garam oksidasiTambahan titanium berfungsi, dengan perawatan panas yang tepat, untuk menstabilkan paduan terhadap sensitisasi terhadap korosi intergranular.Ketahanan Incoloy 825 terhadap korosi umum dan lokal di bawah berbagai kondisi memberikan paduan ini kegunaan luasAplikasi meliputi pengolahan kimia, pengendalian polusi, pemulihan minyak dan gas, produksi asam, operasi pickling, pengolahan ulang bahan bakar nuklir dan penanganan limbah radioaktif.
Sifat luar biasa dari Incoloy 825 adalah ketahanan korosi. dalam mengurangi & kondisi oksidasi, Incoloy 825 tahan korosi umum, lubang & retakan korosi,Korosi intergranular dan retakan korosi teganganHal ini sangat berguna dalam asam sulfat dan fosfor, gas asap yang mengandung belerang, gas asam dan sumur minyak dan air laut.
Incoloy 825 disetujui untuk suhu operasi kapal bertekanan hingga 525C (AS1210, AS4041), 538C (ASME Boiler & Pressure Vessel Code, Bagian I, III, VIII, IX, Kasus 1936, N-188).Fase rapuh dapat terbentuk dalam paduan 825 pada suhu di atas ~ 540C, sehingga biasanya tidak digunakan pada suhu ini, di mana sifat creep-rupture akan menjadi faktor desain.
Komposisi kimia dari Incoloy Alloy 825
Tabel 1.Komposisi kimia dari Incoloy Alloy 825 (ASTM B163 Heat exchanger tube)
Elemen |
% | Elemen | % |
Nikel | 38.0-46.0 | Karbon | 0.05 maksimal |
Kromium | 19.5--23.5 | Mangan | 1.0 maksimal |
Molybdenum | 2.5-3.5 | Sulfur | 0.03 maksimal |
Tembaga | 1.5 --3.0 | Silikon | 0.5 maksimal |
Titanium | 0.6-1.2 | Aluminium | 0.2 maksimal |
Besi | 220,0 menit (~ 33%) |
Sifat tarik dari paduan Incoloy 825
Tabel 2.Sifat ketegangan suhu kamar yang khas (tidak untuk desain. Lihat spesifikasi material atau produk yang relevan untuk nilai desain)
Bentuk |
Kondisi | 00,2% bukti stres MPa |
Kekuatan tarik MPa |
Elong % |
|||
Tabung | Berwarna hitam | 440 | 770 | 35 | |||
Tabung | Ditarik dingin | 880 | 1000 | 15 |
Ketahanan Korosi
Sifat luar biasa dari Incoloy 825 adalah ketahanan korosi. Dalam mengurangi & kondisi oksidasi, Incoloy 825 tahan korosi umum, lubang & retakan korosi,Korosi intergranular dan retakan korosi teganganHal ini sangat berguna dalam asam sulfat dan fosfor, gas asap yang mengandung belerang, gas asam dan sumur minyak dan air laut.
Incoloy 825 dapat dengan mudah diproses panas atau dingin.Untuk ketahanan korosi maksimum bagian yang diproses panas harus stabilisasi annealed sebelum digunakanPaduan ini lebih mudah terbentuk dingin daripada stainless steel.
Pengolahan Panas
Incoloy 825 adalah stabil annealed pada 940C. Struktur paling lunak diperoleh pada 980C. Bagian yang lebih berat dari lembaran, strip dan kawat harus dimatikan untuk menghindari sensitisasi.
Aplikasi
Incoloy 825 adalah bahan pilihan dalam berbagai aplikasi hingga suhu sekitar 550C (1020F),
Kontak Person: Naty Shen
Tel: 008613738423992
Faks: 0086-574-88017980