| Standard: | JIS G4305, JIS G4304 , ASTM A240 | Meterial Grade: | SUS 301, SUS 3001L , SUS 304, SUS304L , SUS316, SUS316L, SUS329J1 |
|---|---|---|---|
| Surface: | BA , 2B, LBA | Hardness: | 1/4H, 1/2H, 3/4H, H, FH |
| Menyoroti: | Strip Baja Tahan Karat JIS G4305,Strip Baja Tahan Karat SUS 304,Strip Baja Tahan Karat ASTM A240 |
||
JIS G4305 SUS 304 Stainless Steel Strip, 1/2H, BA, Aplikasi Otomotif
Yuhong Group sudah memasok strip stainless steel kami ke Sinagpore, Malaysia, Indonesia, Korea, U.A.E., Kolombia, ... SS strip sudah luas digunakan di dapur, Hard Disk komputer, E-rokok, semikonduktor, industri makanan, industri mobil, .... Produk kami sesuai dengan ASTM A240, JIS G4304, JIS 4305, Permukaan sesuai dengan: 2B, BA, LP, Mirror,.... Kekerasan kelas: 1/4H, 1/2H, 3/4H, H, FH.
| Perbaikan permukaan dari kumparan stainless steel | |
|
Perbaikan permukaan
|
Definisi dan Penerapan |
| Tidak, tidak.1 | Permukaan selesai dengan pengolahan panas dan pemurnian atau proses yang sesuai dengan itusetelah penggulingan panas |
| 2D | Hasil akhir setelah pengolahan dingin, dengan perawatan panas, pemurnian atau pengolahan setara lainnya |
| 2B | Akhir setelah penggulung dingin, dengan perawatan panas, pemurnian atau perawatan setara lainnya dan akhirnya dengan penggulung dingin untuk memberikan kilau yang tepat |
| BA | Digulung dingin, terang annealed dan kulit-passed, produk memiliki kecerahan yang sangat baik dan reflektivitas yang baik seperti cermin |
| Tidak, tidak.3 | Dipoli dengan sabuk abrasif dari kerikil#100~#200, memiliki kecerahan yang lebih baik dengan garis kasar diskontinu |
| Tidak, tidak.4 | Dipoli dengan sabuk abrasif dari pasir#150~#180, memiliki kecerahan yang lebih baik dengan garis kasar diskontinu |
| HL | Dipoli dengan sabuk abrasif dari kerikil#150~#320 pada NO.4 finish dan memiliki garis-garis terus menerus |
| 8K | Produk memiliki kecerahan yang sangat baik dan refleksifitas sempurna dapat menjadi cermin |
|
Jenis, Properti Mekanis, Properti Fisik
|
||||||||||||||
| Jenis | Komposisi kimia (%) | Sifat Mekanis | Sifat Fisik | |||||||||||
| KS(JIS) | POSCO | C | Cr | Tidak | Mo | lainnya | Kekuatan Hasil (0,2%) | Kekuatan tarik | Perpanjangan (%) | Kekerasan (Hv) | Panas spesifik J/g °C | Gravitasi Spesifik | Koefisien Ekspansi Termal | Konduktivitas Termal |
| (N/mm2) | (N/mm2) | W/m·°C | W/m·°C | |||||||||||
| (20-100°C) | (100°C) | |||||||||||||
| 409L | 409L | 0.03 | 10.50 ~ 11.75 | - | - | Ti 6xC% ~ 0.75 | 175 ~ | 360 ~ | 25 ~ | ~ 175 | 0.46 | 7.75 | 6.5 | 24.9 |
| - | HIPOS | ~ 0.03 | 12 ~ 14 | - | - | Si ~ 1.3 | 175 ~ | 360 ~ | 22 ~ | ~ 180 | - | - | - | - |
| 410L | 410L | ~ 0.03 | 11.0 ~ 13.5 | - | - | - | 195 ~ | 360 ~ | 22 ~ | ~200 | 0.46 | 7.75 | 9.9 | 25.1 |
| - | 429EM | 0.02 | 13.0 ~ 15.0 | - | - | Si ~ 1.5 | 205 ~ | 400 ~ | 25 ~ | ~ 180 | 0.456 | 7.62 | 10.6 | 20.9 |
| 430 | 430 | ~ 0.12 | 16.0 ~ 18.0 | - | - | - | 205 ~ | 450 ~ | 22 ~ | ~200 | 0.46 | 7.7 | 10.5 | 23.9 |
| 430J1L | 430J1L | ~ 0.025 | 16.0 ~ 20.0 | - | - | N ~ 0.025 | 205 ~ | 390 ~ | 22 ~ | ~200 | 0.46 | 7.7 | 10.4 | 26.2 |
| 430Ti | 430Ti | ~ 0.02 | 19.5 ~ 20.5 | - | - | Ti 0,3 ~ 0.6 | 206 ~ | 422 ~ | 25 ~ | ~ 180 | 0.46 | 7.7 | 10.4 | 26.4 |
| 436L | 436L | ~ 0.025 | 16.0 ~ 19.0 | - | 0.75 ~ 1.5 | Ti, Nb, Zr 8x ((C%+N%) ~ 0.8 | 245 ~ | 410 ~ | 20 ~ | ~ 230 | 0.46 | 7.7 | 9.3 | 23.9 |
| - | 439 | 0.03 | 17.0 ~ 19.0 | - | - | Ti 0,2 ~ 1.0 | 175 ~ | 400 ~ | 22 ~ | ~ 175 | 0.46 | 7.7 | 10.5 | 26.4 |
| - | 441 | ~ 0.03 | 17.5 ~ 18.5 | ~ Satu.0 | - | Si~1.0 Ti 0.1~0.6 Nb 9C+0.3~1.0 | 250 | 430 ~ 630 | 25 ~ | ~ 175 | 0.462 | 7.6 | 10.1 | 27.1 |
| 444 | 444 | ~ 0.025 | 17.0 ~ 20.0 | - | 1.75 ~ 2.5 | Ti, Nb, Zr 8x ((C%+N%) ~ 0.8 | 245 ~ | 410 ~ | 20 ~ | ~ 230 | 0.427 | 7.75 | 11 | 26.8 |
| - | 445NF | ~ 0.015 | 20.0 ~ 23.0 | ~ 0.5 | - | Ti+Nb 10 ((C+N) ~ 0.6 | 245 ~ | 410 ~ | 22 ~ | ~200 | 0.44 | 7.74 | 10.5 | 23 |
| 446M | 446M | 0.015 | 25 ~ 28.5 | ~ 0.3 | 1.5 ~ 2.5 | Ti+Nb 8~(C+N) | 270 ~ | 430 ~ | 20 ~ | ~210 | 0.5 | 7.75 | 11 | 18.84 |
|
Jenis, Sifat Mekanis, Sifat Fisik
|
||||||||||||||
| Jenis | Komposisi kimia (%) | Sifat Mekanis | Sifat Fisik | |||||||||||
| KS(JIS) | POSCO | C | Cr | Tidak | Mo | lainnya | Kekuatan Hasil (0,2%) | Kekuatan tarik | Perpanjangan (%) | Kekerasan (Hv) | Panas spesifik J/g °C | Gravitasi Spesifik | Koefisien Ekspansi Termal | Konduktivitas Termal |
| (N/mm2) | (N/mm2) | W/m·°C | W/m·°C | |||||||||||
| (20-100°C) | (100°C) | |||||||||||||
| 410 | 410 | ~ 0.15 | 11.5 ~ 13.5 | - | - | - | 205 ~ | 440 ~ | 20 ~ | 210 ~ | 0.46 | 7.7 | 9.9 | 24.9 |
| - | 410B | ~ 0.15 | 11.5 ~ 13.5 | 0.6 | - | - | 205 ~ | 440 ~ | 20 ~ | ~210 | 0.46 | 7.75 | 9.9 | 24.9 |
| - | 420N1 | ~ 0.17 | 12.0 ~ 14.0 | - | - | N ~ 0.14 | 225 ~ | 520 ~ | 18 ~ | ~218 | 0.46 | 7.75 | 10.3 | 23.8 |
| 420J2 | 420J2 | 0.26 ~ 0.4 | 12.0 ~ 14.0 | - | - | - | 225 ~ | 540 ~ | 18 ~ | ~ 247 | 0.46 | 7.75 | 10.3 | 23.8 |
| Jenis | Komposisi kimia (%) | Sifat Mekanis | Sifat Fisik | |||||||||||
| KS(JIS) | POSCO | C | Cr | Tidak | Mo | lainnya | Kekuatan Hasil (0,2%) | Kekuatan tarik | Perpanjangan (%) | Kekerasan (Hv) | Panas spesifik J/g °C | Gravitasi Spesifik | Koefisien Ekspansi Termal | Konduktivitas Termal |
| (N/mm2) | (N/mm2) | W/m·°C | W/m·°C | |||||||||||
| (20-100°C) | (100°C) | |||||||||||||
| 329J3L | 329J3L | ~ 0.03 | 21.0 ~ 24.0 | 4.5 ~ 6.5 | 2.5 ~ 3.5 | N 0,08 ~ 0.20 | 450 ~ | 620 ~ | 18 ~ | ~ 320 | 0.4 | 7.8 | 13.7 | 19 |
| 329LD | 329LD | ~ 0.03 | 19.0 ~ 22.0 | 2.0 ~ 4.0 | 1.0 ~ 2.0 | N 0,14 ~ 02 | 450 | 620 ~ | 25 ~ | ~310 | 0.52 | 7.71 | 13.2 | 16.5 |
| Mn 2,0 ~ 4.0 | ||||||||||||||
![]()